I did some SPAMMER cleanup - Report any Posts using the REPORT POST icon.
Hi,Was going to give a call after the holidays with some plating questions as well. Do the choke & secondary flaps get plated? Does the choke flap & shaft need removed from airhorn?Do the tubes need removed from airhorn prior to plating?Thanks
Pic of a finished unit showing the plating process that we use here. The main casting and airhorn are zinc/chromated, the small parts are electroplated.We charge $45 to do a main casting and airhorn, $125 for the whole deal......Cliff